توضیحات
:Product properties
Advantages
High transparency and anti-yellowing, the visual effect is similar to transparent thermoplastic, such as PMMA
Excelent post-processing transparency (polishing, spraying UV high-transmitting oil)
Low release force, good molding accuracy, can print models with high definition and fine details
Features
High transparency and anti-yellowing, suitable for high transparency applications in non-high temperature environment, with imitation acrylic and glass appearance effect, excellent internal transparency which is more suitable for shape and assembly verification, suitable for engineering models with high transparency shell parts, and can also be used to verify exquisite transparency concepts models, such as glasses, high-transparency earphone shells, lampshades, etc.
:Precautions
Kept away from light for a long time and stored in a place with high air humidity. The printer should be covered during printing and avoid indoor light. Please take as much resin as you use
After the model is printed, use high-concentration alcohol to clean it, and cure for 1-2 minutes after with a UV lamp to avoid air humidity affect. The printed resin needs to be stored in a separate bottle and should not be returned to the original bottle
If the UV lamp is irradiated for too long, it can be left for a period of time, and the model will turn yellow. You can also use a microwave oven to remove yellow and red, soak in hot water and put in the microwave for 30 seconds
Post-processing steps: first grinding and polishing, generally from low-mesh sandpaper to high-mesh sandpaper, such as 400 mesh → 600 mesh → 800 mesh (the higher the number of grinding meshes, the higher the transparency of the gloss oil), and then spray after polishing anti-UV high translucent oil to achieve the best transparency effect
مشخصات فنی
Product parameters: Strength: 3 / Toughness : 3 / Forming: 4/ Accuracy : 4/ Speed : 2
: Performance parameters
3D PRINTING PHOTOPOLYMER RESIN : eResin-PMMA Like
Tensile Strength(MPa):58
Flexural Strength(Mpa): 30
Elongation at Break(%): 10%
IZOD Impact Strength/(J/m): 15
Hardness(Shore D) : 70
Viscosity : 300
Density: 1.05-1.15